PARÂMETROS PADRÃO DO CIMENTO PO/PC COM GB175-2007
PRODUCTO | TIPO | TIPO DE ESTUFA | TESTE PADRÕES | |||||
CIMENTO | PO/PC | ESTUFA GIRATÓRIA | GB175-2007 | |||||
TESTE O ARTIGO | UNIDADE | ALVOS IMPERATIVOS (32.5/R) | ALVOS IMPERATIVOS (42.5/R) | ALVOS IMPERATIVOS (52.5/R) | ||||
JUSTEZA | milímetro | ≤10 | ≤10 | ≤10 | ||||
SO3 | % | ≤3.5 | ≤3.5 | ≤3.5 | ||||
MGO | % | ≤5.0 | ≤5.0 | ≤5.0 | ||||
ALCALÓIDE EQ (NA2O+0.658K2O) | % | ≤0.6 | ≤0.6 | ≤0.6 | ||||
ÍNDICE DO CLORETO | % | ≤0.06 | ≤0.06 | ≤0.06 | ||||
GRAU Da FINURA (80UM/45UM) | % | ≤10/≥30 | N.A | N.A | ||||
FINURA (SUPERFÍCIE ESPECÍFICA) | m2/kg | N.A | ≥300 | ≥300 | ||||
PERDA NA IGNIÇÃO | % | ≤5.0 | ≤5.0 | ≤5.0 | ||||
RESÍDUO INSOLÚVEL | % | N.R. | N.R. | N.R. | ||||
TEMPO DO AJUSTE | INICIAL | h/min | ≥00: 45 | ≥00: 45 | ≥00: 45 | |||
FINAL | ≤10: 00 | ≤10: 00 | ≤10: 00 | |||||
RIGIDEZ FLEXURAL | 3 DIAS | Mpa | ≥2.5/3.5 | ≥3.5/4.0 | ≥4.0/5.0 | |||
28 DIAS | ≥5.5 | ≥6.5 | ≥7.0 | |||||
FORÇA COMPRESSIVA | 3 DIAS | ≥10/15 | ≥17/22 | ≥23/27 | ||||
28 DIAS | ≥32.5 | ≥42.5 | ≥52.5 | |||||
China